A fusion procedure relies on the dissolution of a properly oxidized sample in the molten flux. During this procedure, a sub-oxidized sample can be oxidized with a nitrate-based compound. When heated, such oxidizer will promote the full oxidation of your sample in order to ensure a complete dissolution in the flux.
The non-wetting (nwa) agents will avoid the melt sticking on both the crucibles and the molds. Too little nwa could result in dirty crucibles and cracked beads. Our fluxes are available with the additives integrated at the factory. But for method development, an inventory of various additives are convenient tools in any fusion lab.